Cement grouts A and B become unstable above WC of 06 and 08 respectively This means that they exceed the limit of 5 bleed water on the surface after 120 min The extra fineness of cement B could be the reason for the improved stability of the grout – The majority of microfine cement grouts are stable even with a WC of more than 12

As a leading global manufacturer of crushing equipment, milling equipment,dressing equipment,drying equipment and briquette equipment etc. we offer advanced, rational solutions for any size-reduction requirements, including quarry, aggregate, grinding production and complete plant plan. If you are interested in these product, please contact us.